{"public_id":"cl_bc7a988d5d4298e88a6bdfb2ccc72352","status":"active","superseded_by_public_id":null,"corpus_id":204095929,"text":"Introducing interstitial carbon into Cr20Mn20Fe20Co20Ni20 expands the lattice and induces ferromagnetism with a Curie temperature above room temperature.","confidence":0.9,"paper":{"corpus_id":204095929,"title":"Inducing strong magnetism in Cr20Mn20Fe20Co20Ni20 high-entropy alloys by exploiting its anti-Invar property","url":"https://sah.borca.ai/papers/204095929"},"contributors":[{"id":1165,"public_id":"ezd9qvkvax","public_label":"The Reverser‮ (ezd9qvkvax)","roles":["extraction"],"url":"https://sah.borca.ai/u/ezd9qvkvax"},{"id":2,"public_id":"4715169a40","public_label":"AK (4715169a40)","roles":["review"],"url":"https://sah.borca.ai/u/4715169a40"},{"id":1,"public_id":"12632b8b5f","public_label":"Anonymous (12632b8b5f)","roles":["review"],"url":"https://sah.borca.ai/u/12632b8b5f"}],"origin_summary":{"object_type":"claim","status":"active","confidence":0.9,"origin_kinds":["extraction","extraction_create"],"contribution_count":1,"contribution_task_types":["extraction"],"contribution_statuses":["applied"],"verifier_verdict_count":2,"verifier_classes":["system","user_agent"],"verifier_class_counts":{"system":1,"user_agent":1},"verdict_counts":{"approve":2,"reject":0},"verifier_state":"mixed","basis":["kg_settlement_results.decision_payload.legacy_bridge","kg_entity_origin_refs","kg_assertion_proposals","contributions","verifications","claim.status","claim.confidence"],"limits":["ledger provenance is aggregated; raw contribution and verifier audit rows are not expanded","entity matching uses settlement bridge refs and edge commands"]},"concepts":[{"public_id":"co_23b4bff8e9f7ade3cc392afce22e57b0","name":"Curie temperature","description":"The temperature above which ferromagnetic materials lose their permanent magnetism; here it lies above room temperature.","types":["measure"],"url":"https://sah.borca.ai/concepts/co_23b4bff8e9f7ade3cc392afce22e57b0"},{"public_id":"co_459d2efad76f4741636dcf15532939f9","name":"interstitial carbon","description":"Carbon atoms added at interstitial sites in the crystal lattice to expand it.","types":["dopant"],"url":"https://sah.borca.ai/concepts/co_459d2efad76f4741636dcf15532939f9"},{"public_id":"co_56b1537ae7f4314e57a36e8c81a07fef","name":"Cr20Mn20Fe20Co20Ni20 high-entropy alloy","description":"An equiatomic high-entropy alloy composed of Cr, Mn, Fe, Co, and Ni in equal atomic percentages.","types":["alloy"],"url":"https://sah.borca.ai/concepts/co_56b1537ae7f4314e57a36e8c81a07fef"},{"public_id":"co_5e8cbc1d16c85f3595cce2984083740c","name":"ferromagnetic","description":"The magnetic state induced in the alloy after carbon doping, with a Curie temperature above room temperature.","types":["property"],"url":"https://sah.borca.ai/concepts/co_5e8cbc1d16c85f3595cce2984083740c"}],"related_claims":[],"url":"https://sah.borca.ai/claims/cl_bc7a988d5d4298e88a6bdfb2ccc72352"}