The fatigue strength, effects of a notch on the fatigue strength, and fatigue crack growth rate of Ti-15Zr-4Nb-4Ta alloy were compared with those of other implantable metals. Zr, Nb, and Ta are important alloying elements for Ti alloys for attaining superior long-term corrosion resistance and biocompatibility. The highly biocompatible Ti-15Zr-4Nb-4Ta alloy exhibited an excellent balance between strength and ductility. Its notched tensile strength was much higher than that of a smooth specimen. The strength of 20% cold-worked commercially pure (C.P.) grade 4 Ti was close to that of Ti alloy. The tension-to-tension fatigue strength of an annealed Ti-15Zr-4Nb-4Ta rod at 107 cycles was approximately 740 MPa. The fatigue strength of this alloy was much improved by aging treatment after solution treatment. The fatigue strengths of C.P. grade 4 Ti and stainless steel were markedly improved by 20% cold working. The fatigue strength of Co-Cr-Mo alloy was markedly increased by hot forging. The notch fatigue strengths of 20% cold-worked C.P. grade 4 Ti, and annealed and aged Ti-15Zr-4Nb-4Ta, and annealed Ti-6Al-4V alloys were less than those of the smooth specimens. The fatigue crack growth rate of Ti-15Zr-4Nb-4Ta was the same as that of Ti-6Al-4V. The fatigue crack growth rate in 0.9% NaCl was the same as that in air. Stainless steel and Co-Cr-Mo-Ni-Fe alloy had a larger stress-intensity factor range (ΔK) than Ti alloy.
Comparison of Fatigue Properties and Fatigue Crack Growth Rates of Various Implantable Metals
Published 2012 in Materials
ABSTRACT
PUBLICATION RECORD
- Publication year
2012
- Venue
Materials
- Publication date
2012-12-01
- Fields of study
Medicine, Materials Science, Engineering
- Identifiers
- External record
- Source metadata
Semantic Scholar
CITATION MAP
EXTRACTION MAP
CLAIMS
- No claims are published for this paper.
CONCEPTS
- No concepts are published for this paper.
REFERENCES
Showing 1-46 of 46 references · Page 1 of 1
CITED BY
Showing 1-41 of 41 citing papers · Page 1 of 1